Strudex natural rubber screen panels offer two defined hardness choices for mineral screening: 40 and 60 Shore A. The rubber surface provides resilience under impact and repeated contact with abrasive material, making compound selection an important part of the screening-media specification. The softer and firmer options give plant teams a practical basis for comparing surface response against their current wear and blockage problems. Select the panel geometry and connection alongside the rubber grade.
| Availability: | |
|---|---|
| Quantity: | |
305x610 305x305
Strudex natural rubber screen panels offer a defined choice between 40 and 60 Shore A for mineral screening. The natural-rubber surface provides elastic recovery under changing particle contact, while the selected panel geometry presents the openings to the feed. The two hardness options allow the working response to be considered with impact, aperture blockage and wear, rather than treating every rubber panel as the same replacement.
| Parameter | Specification |
|---|---|
| Panel type | Wear-resistant rubber screen panel |
| Rubber material | Natural rubber |
| Rubber hardness options | 40 Shore A / 60 Shore A |
| Nominal module formats | 305 × 305 mm / 305 × 610 mm |
| Fixing category | Pin-type installation |
| Surface behavior | Resilient rubber for repeated impact contact |
A screening panel experiences repeated, changing contact rather than a single static load. Natural rubber can yield locally and recover as particles move away. That resilience provides cushioning under impact and movement around an opening. It is useful only when the complete section remains supported and the aperture geometry continues to deliver the required product. The material and the panel shape therefore need to be selected as one working component.
| Contact condition | What the rubber surface needs to do |
|---|---|
| Repeated particle impact | Accommodate changing contact without losing the intended working shape. Describe particle size, drop and contact concentration, because the same hourly tonnage can reach the panel in very different ways. The support beneath the rubber remains part of this loading system. |
| Sliding abrasive material | Retain useful material around the apertures as particles travel across the face. Inspect opening edges and webs, where wear can change separation before the whole panel is consumed. The objective is a serviceable screening passage rather than surface appearance alone. |
| Particles near the opening size | Allow enough local movement to assist release while maintaining the selected geometry. Feed shape and the narrow dimension of the opening influence whether a particle passes or lodges. Greater flexibility is a selection consideration, not a substitute for the required product specification. |
The 40 Shore A option is softer; the 60 Shore A option is firmer. This is a practical starting point for comparing deformation at the working surface. It does not establish that the firmer grade always resists abrasion better or that the softer grade always prevents blockage. Compound formulation, section thickness and the geometry of the rubber between openings also influence how the panel responds to its particular duty.
The listed model formats are 305 × 305 mm and 305 × 610 mm, with pin-type installation identified for this product. Those formats define module spaces, while the pin pattern, seating and build dimensions establish the installed connection. The grade choice should not obscure those interfaces. A correctly selected rubber material needs the specified support to develop its intended response instead of flexing across an unintended gap.
| Selection objective | Evidence that keeps the decision useful |
|---|---|
| Release lodged material | Identify the particles and the openings involved, then compare blocked area with product grading. Record moisture and near-size content so an easier feed is not credited to the new grade. |
| Retain opening geometry under wear | Keep new-opening reference dimensions and inspect comparable locations. Compare the separated streams with the product requirement, rather than judging the surface only by remaining thickness. |
| Handle a repeated impact zone | Link the panel position to feed trajectory and credible top size. Note cuts, torn webs and any support-related damage separately from gradual abrasive thinning. |
Other rubber properties help explain a candidate grade. Tensile behavior, elongation, tear resistance and abrasion results describe different tests; they should be compared on matching methods and conditions. Their purpose is to characterize the material. A field decision still concerns the complete panel’s ability to remain retained and provide the required separation under representative loading. This avoids converting an isolated laboratory number into a promised operating interval.
For a replacement specification, state the hardness option with the panel drawing, aperture layout, thickness, pin interface and deck position. Include the contact condition that drives the selection. Verification can then cover the agreed grade identification and critical dimensions, while the operating record shows whether the chosen natural-rubber configuration continues to meet the plant’s screening objective.